Atomic Layer Deposition for Energy Conversion and Storage Applications - read free eBook in online reader or directly download on the web page. Select files or add your book in reader. Download and read online ebook Atomic Layer Deposition for Energy Conversion and Storage Applications write by Sebastian Häringer. This book was released on 2024. Atomic Layer Deposition for Energy Conversion and Storage Applications available in PDF, EPUB and Kindle.
Atomic Layer Deposition in Energy Conversion Applications
Atomic Layer Deposition in Energy Conversion Applications - read free eBook in online reader or directly download on the web page. Select files or add your book in reader. Download and read online ebook Atomic Layer Deposition in Energy Conversion Applications write by Julien Bachmann. This book was released on 2017-05-30. Atomic Layer Deposition in Energy Conversion Applications available in PDF, EPUB and Kindle. Combining the two topics for the first time, this book begins with an introduction to the recent challenges in energy conversion devices from a materials preparation perspective and how they can be overcome by using atomic layer deposition (ALD). By bridging these subjects it helps ALD specialists to understand the requirements within the energy conversion field, and researchers in energy conversion to become acquainted with the opportunities offered by ALD. With its main focus on applications of ALD for photovoltaics, electrochemical energy storage, and photo- and electrochemical devices, this is important reading for materials scientists, surface chemists, electrochemists, electrotechnicians, physicists, and those working in the semiconductor industry.
Atomic Layer Deposition in Energy Conversion Applications
Atomic Layer Deposition in Energy Conversion Applications - read free eBook in online reader or directly download on the web page. Select files or add your book in reader. Download and read online ebook Atomic Layer Deposition in Energy Conversion Applications write by Julien Bachmann. This book was released on 2017-03-15. Atomic Layer Deposition in Energy Conversion Applications available in PDF, EPUB and Kindle. Combining the two topics for the first time, this book begins with an introduction to the recent challenges in energy conversion devices from a materials preparation perspective and how they can be overcome by using atomic layer deposition (ALD). By bridging these subjects it helps ALD specialists to understand the requirements within the energy conversion field, and researchers in energy conversion to become acquainted with the opportunities offered by ALD. With its main focus on applications of ALD for photovoltaics, electrochemical energy storage, and photo- and electrochemical devices, this is important reading for materials scientists, surface chemists, electrochemists, electrotechnicians, physicists, and those working in the semiconductor industry.
Three Dimensional Nanoarchitectures by Atomic Layer Deposition for Energy-related Applications
Three Dimensional Nanoarchitectures by Atomic Layer Deposition for Energy-related Applications - read free eBook in online reader or directly download on the web page. Select files or add your book in reader. Download and read online ebook Three Dimensional Nanoarchitectures by Atomic Layer Deposition for Energy-related Applications write by Zhaodong Li. This book was released on 2016. Three Dimensional Nanoarchitectures by Atomic Layer Deposition for Energy-related Applications available in PDF, EPUB and Kindle. Atomic layer deposition (ALD) is a cyclic, multi-step thin film chemical vapor deposition process based on sequential self-limiting surface reactions. It has been widely applied for synthesizing various three dimensional (3D) nanoscale morphologies. Recently, based on ALD process, a surface-reaction-limited pulsed chemical vapor deposition (SPCVD) technique was developed for 3D hierarchical branched nanowire (NW) architecture with super high surface area density and good electronic transport properties. This new ALD-based nanomanufacturing technique demonstrated great potential to conduct large-area and low-cost fabrication of high-density 3D nanomaterials for energy harvesting and storage applications, such as photoelectrochemical (PEC) water splitting, solar cells, batteries and supercapacitors. In this dissertation, a series of experimental work is presented regarding fundamental understandings and rational controls of the SPCVD process in branched nanorod (NR) synthesis, as well as the application potentials of 3D branched nanowire architectures. First, the composition control ability of SPCVD was studied on nitrogen-doped TiO2 NRs to overcome the intrinsically visible light absorption constrains of metal oxide semiconductors. Second, to further improve the porosity and surface area while maintain good redox reaction kinetics, several 3D cellulose nanofibers (CNFs) templated fibrous TiO2 nanoarchitectures were synthesized. By integrating the strong capillary property of CNF film, the capillary PEC and capillary photocatalytic systems were developed by performing water redox reactions outside of the body of electrolyte with enhanced reaction kinetics and higher efficiency. At last, SPCVD was applied to the growth of high-density vanadium oxide (VOx) NR branches on Si NW backbones. Such a 3D hierarchical VOx/Si NW structure exhibited enhanced performance as a supercapacitor. These achievements open a new avenue of ALD for large-area, low-cost, and green fabrication of materials, which would be used in solar energy conversion and electrical energy storage.
Atomic Layer Deposition for Electrochemical Applications
Atomic Layer Deposition for Electrochemical Applications - read free eBook in online reader or directly download on the web page. Select files or add your book in reader. Download and read online ebook Atomic Layer Deposition for Electrochemical Applications write by James Steven Daubert. This book was released on 2017. Atomic Layer Deposition for Electrochemical Applications available in PDF, EPUB and Kindle.